流年
:因为报检都是下午了,如果打磨还来得及,但是如果反冲,清洁就来不及做。所以,如果这个不影响质量就OK了
(2013-12-05 10:11)
参考sspc sp10 2.1.1
2.1.1 Acceptable variations in appearance that do not
affect surface cleanliness as defined in Paragraph 2.1 include
variations caused by the type of steel, original surface condition,
thickness of the steel, weld metal, mill or fabrication marks,
heat treating, heat-affected zones, blasting abrasives, and
differences because of blasting technique.
如果真的遇到一定要纠结在这个问题上的船东,规范也不管的那种,想使外观看起来好看也很简单,办法我就不说了,你去问问冲砂代班,都懂的。